| Peak Forward Anode voltage | 70 | kV max |
| Peak Forward Anode current | 15 | kA max |
| Peak reverse anod current | 10 | kA max |
| Average anode current | 5.0 | A max |
| Rate of rise of current | > 300 | kA/us |
| Jitter | 1.0 | ns |
| Pulse repetition rate | 2000 | pps |
| Cathode | barium aluminate impregnated tungsten | |
| Cathode heater voltage | 6.3 +- 0.3 | V |
| Cathode heater current | 37.5 | A |
| Reservoir heater voltage | 6.3 +-.3 | V |
| Reservoir heater current | 7.0 | A |
| Tube heating time | 10.0 | min |